If you 3D print your own LEGO-compatible bricks, you get parts that fit and function surprisingly well—but they won’t be identical to real LEGO. The studs, tubes, and clutch power (the grip between bricks) depend on precise tolerances that consumer 3D printers can only approximate, so expect a tighter or looser fit, rougher surfaces, and lower strength than injection-molded originals.
Formula
This calculator works out your average pace and speed for a run, ride, or walk. You enter the finish time (in minutes) and the distance (in kilometers), and it returns your average pace in minutes per kilometer and your average speed in kilometers per hour.
The formulas are:
- Pace = Time ÷ Distance (min/km)
- Speed = Distance ÷ (Time ÷ 60) (km/h)
Where:
- Time (t) is the total time in minutes (e.g., 50 min)
- Distance (d) is the distance in kilometers (e.g., 10 km)
- Pace is the time it takes to cover one kilometer
- Speed is the distance covered in one hour
Worked Example
Using the default values from the calculator above (t = 50 minutes, d = 10 km):
- Pace = 50 ÷ 10 = 5.00 min/km
- Speed = 10 ÷ (50 ÷ 60) = 10 ÷ 0.8333 = 12.00 km/h
So a 10 km run in 50 minutes gives an average pace of 5 minutes per kilometer and an average speed of 12 km/h.
Why 3D Printing LEGO Bricks Is Different
LEGO bricks are made by injection molding ABS plastic at high pressure in precision steel molds. The molds are machined to tolerances of about 5 micrometers (0.005 mm) on critical surfaces. Consumer 3D printers (FDM/FFF) typically achieve layer resolutions of 0.1–0.3 mm, which is 20–60 times coarser. That difference alone explains most of the fit issues you’ll encounter.
Also, 3D printing builds parts layer by layer, so the surface is not smooth but has visible ridges (layer lines). These ridges catch on the inner walls of other bricks, increasing friction and making assembly harder. The plastic is also weaker along the layer lines, so a printed brick can split if you force it onto a stud.
What Works and What Doesn’t
In practice, simple parts like 2×4 bricks, 1×2 plates, and flat tiles print reasonably well. The key is to print with the studs facing up and to calibrate your printer’s extrusion rate carefully. Here’s what typically happens:
- Studs fit: The stud diameter (about 4.8 mm) is forgiving; most printers can hit that within 0.2 mm.
- Clutch power varies: The friction that holds bricks together comes from the interference fit between the stud and the tube underneath. If your printer over-extrudes, the fit is too tight; if under-extrudes, too loose.
- Layer lines cause squeaking: The rough surface makes a grinding noise when you push bricks together, and it can scrape off tiny plastic shavings.
- Thin walls break: The walls of a brick are about 1.2 mm thick. With a 0.4 mm nozzle, that’s only 3 perimeters. If the layer adhesion is poor, the wall can crack.
How to Get the Best Results
To maximize the chance of printing usable bricks, follow these tips:
- Use a 0.2 mm layer height or finer (0.1 mm gives smoother sides but doubles print time).
- Print with ABS or PETG if possible. PLA is easier but more brittle and less heat-resistant.
- Calibrate your extruder steps and flow rate. Print a test cube and measure the wall thickness—adjust until you get exactly the nominal value.
- Print at a lower speed (30–40 mm/s) to improve layer adhesion.
- Add a small horizontal expansion (e.g., -0.1 mm) in your slicer to compensate for over-extrusion on outer walls.
- Use a brim or raft if the brick has a small footprint, to prevent warping.
Common Problems and Fixes
- Too tight: If bricks are hard to push together, reduce flow rate by 5–10% or increase horizontal expansion to -0.2 mm.
- Too loose: If bricks fall apart, increase flow rate slightly or print a test with a 0.15 mm layer height.
- Warping: ABS shrinks as it cools. Use a heated bed at 100–110°C and an enclosure, or switch to PETG.
- Stringing: Retraction settings matter. For PLA, start with 5 mm retraction at 40 mm/s; for PETG, 6 mm at 30 mm/s.
- Layer splitting: Increase nozzle temperature by 5–10°C and reduce cooling fan speed to 50% or less for ABS/PETG.
Comparisons: 3D Printed vs. Real LEGO
| Property | Real LEGO | 3D Printed (FDM) |
|---|---|---|
| Surface finish | Smooth, glossy | Rough, matte, layer lines |
| Dimensional accuracy | ±0.005 mm | ±0.1–0.3 mm |
| Clutch power | Consistent, ~15 N | Varies, often 5–20 N depending on settings |
| Strength | High (injection-molded ABS) | Lower, anisotropic (weak along layers) |
| Cost per 2×4 brick | ~$0.10 (bulk) | ~$0.20–$0.50 in filament plus electricity |
Safety and Material Considerations
Most 3D printing filaments are safe to handle, but ABS emits styrene fumes when heated. Use in a well-ventilated area or with an enclosure. PLA is food-safe only if the print is not porous and you use a dedicated nozzle, but it’s not recommended for children’s toys because it can harbor bacteria in layer lines. PETG is a good compromise: strong, low odor, and more flexible than PLA.
Also, printed bricks are not as durable as injection-molded ones. They can break if dropped on a hard floor or if a child steps on them. Always supervise young children with printed parts, as small broken pieces could be a choking hazard.
Frequently Asked Questions
Will 3D printed LEGO bricks work with real LEGO?
Yes, most will fit, but the clutch power may be inconsistent. You may need to adjust your printer settings to get a snug fit. Some bricks may be too tight or too loose, so test a few before printing a large batch.
What is the best filament for LEGO-compatible bricks?
ABS is the closest to real LEGO in feel and durability, but it’s tricky to print. PETG is easier and nearly as strong. PLA is the simplest but more brittle and less heat-resistant.
How long does it take to print a 2×4 brick?
With a standard 0.4 mm nozzle and 0.2 mm layer height, a 2×4 brick (about 32×16×9.6 mm) takes roughly 15–25 minutes. Smaller plates can take 5–10 minutes.
Can I use a resin printer for LEGO bricks?
Resin printers can produce smoother, more accurate parts, but resin is brittle and not flexible. The bricks may crack under stress. Also, resin requires post-curing and is more expensive per part.
Why do my printed bricks crack along the layers?
Layer adhesion is weak if the nozzle temperature is too low or the cooling fan is too high. Increase temperature by 5–10°C, reduce fan speed, and ensure your bed is level.
Is it legal to 3D print LEGO-compatible bricks?
Yes, for personal use. The patent on the classic brick expired long ago. However, the LEGO logo and specific minifigure designs are trademarked, so selling copies of those is not allowed.
Related
Formula used
in t | Finish time | min | 50 | 0 in d | Distance | km | 10 | 0 out pace | Average pace | min/km | t / d | 2 out speed | Average speed | km/h | d / (t / 60) | 2
Each line is one input (in, sel, list) or one result (out: label, unit, formula, decimals). How the calculators work
Method: the standard formula for this calculation, rounded as each result states. See how the calculators work or report an error.